华电技术 ›› 2019, Vol. 41 ›› Issue (7): 67-69.

• 技术交流 • 上一篇    下一篇

水溶纸对主蒸汽品质的影响和分析

  

  1. 润电能源科学技术有限公司, 郑州〓450000

  • 出版日期:2019-07-25 发布日期:2019-08-08

Influence and analysis of water soluble paper on main steam quality

  1. Rundian Energy Science and Technology Company Limited, Zhengzhou 450000, China

  • Online:2019-07-25 Published:2019-08-08

摘要:

某发电公司为防止过热器氧化皮剥落引起过热器爆管事故,在机组检修期间,对其进行割管检查。在使用氩弧焊恢复过程中,为使焊缝处于氩气保护氛围,使用上海某科技公司生产的“速溶型水溶纸”对焊口两端进行了封堵。机组并网后主蒸汽氢电导率多次出现超标现象,经分析,主要原因是机组启动前没有对过热器进行充分的冲洗,该速溶型水溶纸氯化物和硫酸盐等含量过高,残存的水溶纸在机组启动后持续释放出氯化物和硫酸盐等杂质离子导致主蒸汽氢电导率出现异常偏高。对此提出了防范措施,以确保主蒸汽品质达标。

关键词:

font-size: 10.5pt, mso-spacerun: 'yes', mso-font-kerning: 1.0000pt">水溶纸, 氩弧焊, 主蒸汽, 氢电导率, 极限摩尔电导率, 羧甲基纤维素

Abstract:

In order to prevent superheater tube burst caused by oxide coat peeling in a power generation company, pipe cutting inspection was carried out during unit overhaul.In the recovery process with argon arc welding, a special type of instant watersoluble paper” was used to seal both ends of the weld in order to make the weld be protected by argon atmosphere.The hydrogen conductivity of the main steam of the unit repeatedly exceeded the standard after being connected to the grid.The main reason is that the superheater had not been washed sufficiently before the unit startup.The content of chloride and sulfate in the instant watersoluble paper is too high.The residual watersoluble paper continuously releases impurity ions such as chloride and sulfate after the unit startup.It is the main reason for the abnormal high hydrogen conductivity of main steam.Preventive measures are put forward to ensure that the quality of main steam reaches the standard.

Key words:

font-size: 10.5pt, mso-spacerun: 'yes', mso-font-kerning: 1.0000pt">water soluble paper;argonfont-size: 10.5pt, mso-spacerun: 'yes', mso-font-kerning: 1.0000pt">font-size: 10.5pt, mso-spacerun: 'yes', mso-font-kerning: 1.0000pt">arc welding;main steam;hydrogen conductivity;limiting molar conductivity;carboxymethyl cellulose