Abstract: The serious ash fouling fault was happened in air preheater of boiler No.4 of Xinjiang Huadian Hongyanchi Power Generation Corporation Limited, which influenced on the stability of pulverized coal combustion and the safety of electrostatic precipitator, and the boiler was be compelled to shut down for cleaning the deposited ash manually. The reason of ash fouling in air preheater was analyzed, some detailed preventive measures were put forward, and the problems of ash fouling in air preheater and low temperature corrosion were solved.
Key words: air preheater, ash fouling, low temperature corrosion
XIAO Xingquan. Analysis of ash fouling of air preheater and solving measures[J]. Huadian Technology, 2009, 31(2): 22-23.
/ Recommend
Add to citation manager EndNote|Ris|BibTeX
URL: https://www.hdpower.net/EN/
https://www.hdpower.net/EN/Y2009/V31/I2/22
Optimization of air preheater leakage control system in 670MW unit
Study on the distribution and optimization control of SCR denitration system flue gas flow field
Operation optimization an SCR denitration system in a coalfired power plant